http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014234637-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d44b532d6aa1bf173c57dad794450202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_59d6e2cb7b092787a4f5db2a3277e536 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8cbc6d052230bb4b1ac2c35b8803cf53 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31663 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 |
filingDate | 2011-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_841d01b1e4c41fc55065d5dd1e214a4b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_440c4f09737099076c47c352fd057d4e |
publicationDate | 2014-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2014234637-A1 |
titleOfInvention | Optical article comprising a temporary antifog coating based on sorbitan surfactants |
abstract | An optical article includes a substrate having a main surface coated with an antireflection coating and, directly contacting the antireflection coating, a precursor coating of an antifog coating obtained through the grafting on the antireflection coating of at least one compound B bearing a polyoxyalkylene group, the coating precursor of the antifog coating being coated with a surfactant film so as to form an antifog coating. The surfactant film contains at least one surfactant A having a sorbitan ring hydroxyl groups functionalized with OH-terminated polyoxyalkylene groups and R1 groups of formula: —(R d O) z —(Y) n2 —R′, in which R d is an alkylene group, z is an integer >1, Y is a divalent group, n2 is 0 or 1 and R′ is a saturated hydrocarbon group having 12 to 1 9, preferably 1 3 to 19 carbon atoms. Surfactants A provide a visual indication whether or not the antifogging effect will still be long-lasting. |
priorityDate | 2011-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |