Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2f8fe6b6115a7e5ede9984cde9aa6191 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-288 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1651 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1658 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1692 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1607 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-31 |
filingDate |
2012-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6dd32e8e756597e51bd9e4f8641d33a1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c182f24a9e46d9fac82262488176adf |
publicationDate |
2014-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2014161972-A1 |
titleOfInvention |
Method for forming conductive film at room temperature |
abstract |
A method for forming a conductive film at room temperature is provided and includes steps of: adding AgNO 3 into a first solution of dodecanoic acid; dropping n-butylamine and a diluted aqueous solution of a reducing agent into the first solution in turn, so as to initially obtain the dodecanoate-protected silver nanoparticles as a capping ligand; then using cyclohexane as a solvent to apply the silver nanoparticles onto a surface of a substrate to form a patterned film of silver nanoparticles; and finally immersing the substrate into a high concentrated aqueous solution of a reducing agent to chemically reduce the patterned film of silver nanoparticles into a conductive silver film. Thus, a patterned film or circuit can be conveniently and rapidly formed, and the silver nanoparticles can be applied to flexible substrates with low material cost and temperature sensitivity. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2698739-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018040429-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018512267-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018033620-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105022103-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2731839-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114477152-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10892160-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015217374-A1 |
priorityDate |
2012-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |