http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014148556-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7783f9d4cf4d727bdb335e27a2da3634 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e09fa74679e9233d1d8bd9ec98b312d2 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2201-012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-024 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-0373 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-48 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-48 |
filingDate | 2011-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0641319b768cac4444aad3c269d8d90d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_516233fddc05fb983460664638880d05 |
publicationDate | 2014-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2014148556-A1 |
titleOfInvention | Method for preparing phosphorus-containing polyphenylene oxide resin with low molecular weight |
abstract | Disclosed is a method for preparing a phosphorus-containing polyphenylene oxide resin with a low molecular weight, comprising the steps of: step 1: providing a phosphorus-containing phenolic compound and a raw polyphenylene oxide resin having a number-average molecular weight of more than 10000; step 2: dissolving the raw polyphenylene oxide resin into a solvent to make a solution of the raw polyphenylene oxide resin; step 3: adding the phosphorus-containing phenolic compound to into the solution of the raw polyphenylene oxide resin; step 4: introducing an initiator, and carrying out a re-dispersing reaction at a reaction temperature of above 60° C. under the effect of the initiator; and step 5: after the reaction is finished, the product obtained being phosphorus-containing polyphenylene oxide resin with a low molecular weight, the number-average molecular weight thereof being 1000-6000. n By dispersing the phosphorus-containing phenolic compound into the solution of polyphenylene oxide resin, and carrying out the re-dispersing reaction in the presence of the initiator to prepare the phosphorus-containing polyphenylene oxide resin with a low molecular weight, the obtained phosphorus-containing polyphenylene oxide resin with a low molecular weight is convenient to process, and suitable for use as the matrix resin of composite materials for high-frequency circuit boards or as an additive component for other polymeric materials. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10233365-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107266685-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015351237-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10104769-B2 |
priorityDate | 2011-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 128.