abstract |
Methods are provided for fabricating a solution-processed metal and mixed-metal selenide semiconductor using a selenium (Se) film layer. One aspect provides a conductive substrate and deposits a first Se film layer over the conductive substrate. A first solution, including a first material set of metal salts, metal complexes, or combinations thereof, is dissolved in a solvent and deposited on the first Se film layer. A first intermediate film comprising metal precursors is formed from corresponding members of the first material set. In one aspect, a plurality of intermediate films is formed using metal precursors from the first material set or a different material set. In another aspect, a second Se film layer is formed overlying the intermediate film(s). Thermal annealing is performed in an environment including hydrogen (H 2 ), hydrogen selenide (H 2 Se), or Se/H 2 . The metal precursors are transformed in the intermediate film(s), and a metal selenide-containing semiconductor is formed. |