http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014106075-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4227fc2692c2ba906cfbaa538309934d |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-792 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6229 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6258 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6254 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-246 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 |
filingDate | 2012-05-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0680c1d262492c0dbb26cee026d7224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6975af616f884cfc62fa1b5e2ee1d970 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8443a6a3d54993a4c69aeede12289928 |
publicationDate | 2014-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2014106075-A1 |
titleOfInvention | Two-component coating compositions |
abstract | Two-component coating compositions include: A) a cross-linkable binder compound having at least one functional group reactive towards isocyanate groups, B) a cross-linking agent having at least one free isocyanate group and C) a catalyst component comprising C1) a catalyst for the for the curing reaction between the functional groups of component A) and the isocyanate groups of component B), said catalyst being an organo-metal compound, and C2) an oligomeric or polymeric binder compound having a glass transition temperature Tg of ≧about 20° C., measured by DSC (differential scanning calorimetry) at a heating rate of 10 K/min. The glass transition temperature Tg of the binder compound C2) is above the temperature at which the two-component coating composition is applied, preferably about 10° C. above the temperature at which the two-component coating composition is applied. |