abstract |
A method for producing a pressure-sensitive adhesive layer-carrying optical film includes the step of applying, over the optical film, a coating liquid for anchor layer comprising a mixed solvent comprising 10 to 100% by weight of water and 90 to 0% by weight of an alcohol, and a polyoxyalkylene-group-containing polymer so as to give an applied-coat thickness before drying of 20 μm or less; and next drying the workpiece under drying conditions satisfying both of the following requirements (1) and (2):n (1) the drying temperature T is from 40 to 70° C., and (2) a value obtained by multiplying the drying temperature T (° C.) by the drying period H (seconds), T×H, satisfies: nn 400≦( T×H )≦4000,n n thereby removing the mixed solvent to form the anchor layer. |