http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013324656-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e7725c83336e5f764a30136b9ba66bd6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_624ec06788fcbcb5b945d854eb3fbd32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4b6c496ba16056a1431fcd4fc2ac8bf8 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F297-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F297-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F293-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F293-00 |
filingDate | 2012-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_023d3b4cb3b0e92ce4b74e977035b068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f44db9797aa8dfb692520e6b848d96ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e5253599b1c2e79a54b293ba5b87d25a |
publicationDate | 2013-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2013324656-A1 |
titleOfInvention | Hydrogenated block copolymer and composition comprising same |
abstract | Provided are a block copolymer and a thermoplastic elastomer composition each of which is excellent in both tensile strength and elastic recovery, and has good abrasion resistance. Specifically, provided are a hydrogenated block copolymer, which is obtained by hydrogenating a block copolymer having two or more polymer blocks (a) each containing a structural unit derived from an aromatic vinyl compound and one or more polymer blocks (b) each containing structural units derived from isoprene and 1,3-butadiene, in which the hydrogenated block copolymer has a crystallization peak temperature (Tc) defined as described below of −3 to 15° C., and a thermoplastic elastomer composition containing the hydrogenated block copolymer: (crystallization peak temperature (Tc)) a peak top temperature of an exothermic peak observed when the temperature of a sample is increased from 30° C. to 150° C. at a rate of temperature increase of 10° C./min and then the sample is cooled to −100° C. at a rate of temperature decrease of 10° C./min, the peak top temperature being measured with differential scanning calorimeter (DSC), is defined as the crystallization peak temperature (Tc). |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9631084-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11345788-B2 |
priorityDate | 2011-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 208.