Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44b2ac87aeadb161b83426d9cf6c4bdc |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-70 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0471 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0564 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0569 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-134 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0564 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-134 |
filingDate |
2013-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3df100d4a2e76fadaa4593f03fce378d |
publicationDate |
2013-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2013260227-A1 |
titleOfInvention |
Lithium-ion secondary battery |
abstract |
The negative electrode is formed from silicon, an amount of heat generation in a negative electrode, which is measured by a differential scanning calorimeter within a range of 210 to 380° C. during full charge, is 850 J/g or less, and a cyclic carbonate including ethylene carbonate and a chain carbonate which has a chemical formula expressed by R 1 —O—CO—OR 2 , and in which R 1 and R 2 represent an alkyl group having a carbon number of 2 or more are used for an electrolytic solution. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2022093982-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3905415-A4 |
priorityDate |
2012-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |