Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ac575e4e8daca81cf4400e704efa37b8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c97f90ab12b35b650d5fd039ed7a41a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3afc191e0142532ebe8e259bdd5f8ddb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133331 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-03 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133308 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1333 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1333 |
filingDate |
2011-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d22abe44dc3ede796c62ef67cf564636 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_441ecbd45b08c14875f1cf7e6a67473f |
publicationDate |
2013-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2013222720-A1 |
titleOfInvention |
Method for manufacturing liquid crystal display device provided with front plate, and liquid crystal display device provided with front plate |
abstract |
The present invention provides a method for manufacturing a liquid crystal device having no wrinkles and distortion between a hard coat layer and a base material film, and no peeling of the hard coat layer. This method stacks a sealing layer having an ultraviolet curable adhesive; a front plate composed of a glass or an acrylic resin; an adhesive layer; and a base material film, which has a resin layer containing an adhesion improving agent, and a hard coat layer on the film surface. The resin layer contains 0.005-0.5 parts of the per 100 parts of a binder resin. The adhesive improving agent has an absorption maximum peak at a wavelength of 260-400 nm at the time of curing the sealing layer by applying ultraviolet rays from the hard coat layer side. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016131931-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106094061-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016231972-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11163132-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10133106-B2 |
priorityDate |
2010-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |