Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a2fe7fc4a2e4f4f1721b16baa6c402d7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_189d98822edc845d427473344adda7c5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_294881271413951a95f284b588a68e66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a33d53ffdc9ae8a6bb9fda9ead0bff15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d4cb567b804bb24017152b6fc412fcf6 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0037 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-122 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0569 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0568 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0567 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0567 |
filingDate |
2011-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d55589c9acd19cc52f07738e075c44d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44f941beb557b9398170fdc5cbb681cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df9d34261d42b3eebe37d74b62d0aa7e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bcd681cf409c7d671e0f0f3409d72b62 |
publicationDate |
2013-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2013202972-A1 |
titleOfInvention |
Electrolyte and secondary battery |
abstract |
A secondary battery capable of decreasing progression temperature of a precipitation-dissolution reaction of aluminum is provided. A cathode 11 and an anode 12 are separated from each other by a separator 13 . An electrolyte with which the separator 13 is impregnated contains an alkyl sulfone (R1—S(═O) 2 —R2: each of R1 and R2 represents an alkyl group) and a solvent (having a specific dielectric constant of 20 or less) together with an aluminum salt. A content of the solvent is equal to or larger than 30 mol % and is less than 88 mol %, and a mol ratio (a content of the aluminum salt/a content of the alkyl sulfone) is equal to or larger than 4/5 and is less than 7/3. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108630895-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018277851-A1 |
priorityDate |
2010-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |