abstract |
The present invention relates to a method for consecutively producing at least two different polyethylene resins in one slurry loop reactor, comprising producing a first polyethylene resin in the presence of a Ziegler-Natta and/or a Chromium catalyst, and consecutively producing a second polyethylene resin in the presence of a metallocene catalyst, characterized in that the ratio of the melt flow index of the first produced polyethylene resin to the melt flow index of the second produced polyethylene resin is at least 0.3. |