Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_edf507cc3aa76c71fa846fd04f92849f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_70dc6cac49fd2cc1b81d24536eef02d1 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-3684 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-68 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-36 |
filingDate |
2011-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_536d3a1bd38387b7f792e06f7702d059 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8eccbfa863ccf6d29019df42449dea1b |
publicationDate |
2012-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2012295032-A1 |
titleOfInvention |
Coating composition and coating film forming method |
abstract |
The present invention relates to a coating composition containing a colored aluminum pigment and a titanium oxide pigment, wherein in the case where a coating film formed from the coating composition is illuminated at 45 degrees with respect to the surface of the coating film, a ratio of lightness L* of light observed at 45 degrees with respect to specularly reflected light, relative to lightness L* of light observed at 110 degrees with respect to specularly reflected light is within a range of 1.00 to 1.50. The invention further relates to a method for forming a coating film, including steps of applying the above-described coating composition to a substrate; and further applying a clear coating composition thereto. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11548029-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11407210-B2 |
priorityDate |
2010-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |