abstract |
A method produces an adhesive tape having a textile carrier and a pressure-sensitive adhesive coated on one side thereof. A shear viscosity of the pressure-sensitive adhesive, at a temperature of 25° C. during coating from dispersion, is 200 to 100 000 Pa*s at a shear rate of 10 −2 s −1 and is 0.1 to 10 Pa*s at a shear rate of 100 s −1. |