Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e37ed55aa3c25e88040247c18bc2b21b |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2211-186 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-203 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0091 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-07 |
filingDate |
2010-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f6c55bf09112deb74e128832809a455 |
publicationDate |
2012-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2012214921-A1 |
titleOfInvention |
Production method of thermoplastic resin composition, molded body, and light emission body |
abstract |
Disclosed is a production method of a thermoplastic resin composition comprising: compounding 0.001 to 50 parts by mass of a metal complex (B) with respect to 100 parts by mass of a thermoplastic resin (A), and kneading it under a condition of a kneading temperature of 225 to 300° C. and of a kneading time of 0.5 to 20 minutes, wherein a metal of the metal complex (B) is a metal except for zinc; a molded body obtained by molding the thermoplastic resin composition which is obtained by the production method; and a light emission body using the molded body. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10934482-B2 |
priorityDate |
2009-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |