Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5f038d86658687ad8352a9f737688b8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6e331ebfd57dacf0b7787f7b987dac18 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2848 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2891 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2433-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-408 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2203-318 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-22 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-22 |
filingDate |
2011-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b589b8ff21fad651febf3264dcf79f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a009d8916d8cd4388ab623e4c3ac2b4f |
publicationDate |
2012-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2012171482-A1 |
titleOfInvention |
Adhesive composition and optical member using the same |
abstract |
An adhesive composition and an optical member using the same, the adhesive composition including an acrylic resin; an isocyanate cross-linking agent; and a carbodiimide cross-linking agent, wherein the adhesive composition exhibits a creeping distance of about 100 μm or less when the composition attached to a glass substrate with a bonding area of about 1.5 cm×1.5 cm is left at about 22° C. and about 50% RH for about 3 days and is subjected to a load of about 10 gf/mm 2 for about 1,000 seconds, and a storage modulus of about 1×10 5 to about 1×10 7 Pa at about 10 Hz and about 30° C. under conditions in which a sample has a thickness of about 1 mm and an elongation of about 10%. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016062028-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11787985-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021284878-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015044945-A |
priorityDate |
2010-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |