Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5fe35cc39dfbe2b82e4660e848e0f6e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8ed912e0ab3419f24b82b8176989f9ab http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efe1bb62e267015ff08ff675e6f89538 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b806f263e9253425625b49bbcb34dfe2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-54 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-05 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B9-00 |
filingDate |
2011-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e281d4065c87c58956d682c4818f03e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d04aff00b2398ccb5ff55994b8a5adf6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da5eaa22a40982e1c72e0325eb4b6f43 |
publicationDate |
2012-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2012126438-A1 |
titleOfInvention |
Process and System for Fabrication and Surface Modification of Colloidal Carbon Spheres in Supercritical Media |
abstract |
A process for producing monodispersed carbon spheres comprising the steps of mixing supercritical-carbon dioxide fluid under pressure with a solvent in an inert atmosphere; heating the mixture in to a temperature to carbonise the solvent; and modulating the pressure to the heated mixture to produce carbon spheres. Subsequent addition of an organometallic precursor can be used to induce the nucleation and growth of nanocrystals across the surface of the spheres. |