abstract |
To provide a toner, containing: a crystalline polyester resin; and a non-crystalline polyester resin, wherein the crystalline polyester resin has a melting point of 60° C. to 80° C., and wherein the toner satisfies the relationship represented by the following formula: (W1−W1′)/W1<0.50, where W1 is a temperature width at a 1/3 height of a height of an endothermic peak of the crystalline polyester resin at the time of an initial temperature elevation on a DSC curve of the toner as measured by differential scanning calorimetry, and W1′ is a temperature width at a 1/3 height of a height of an endothermic peak of the crystalline polyester resin after the toner has been heated at 50° C. for 24 hours. |