http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2012049406-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2707056d594790a62947ee030653e6f8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bccfa781efb475dfbb851764561ae486
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fbfb154f7a21e1bc6d8006f7b6850cde
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_61c420150f71a21674eab8665ba56c1b
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f20e9721e1396eed4ff85a936cd362f9
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2331-021
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2978
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-919
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D7-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-05
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D03D13-008
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-605
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-05
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-60
filingDate 2011-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ed404527c238c7de7bb814f4cc42abc
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d39a9d467d272da66401479ff7d82d5
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01404b7c6470a10fa5f4ad74f87d49c4
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8400a6d3cd3c9816f4ecccd6b60b918
publicationDate 2012-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber US-2012049406-A1
titleOfInvention Para-aramid fiber and method of preparing the same
abstract An aramid fiber and a method of producing the same is disclosed, which is capable of realizing high surface uniformity and improved tensile strength and elongation property, wherein the method comprises preparing an aromatic polyamide by polymerizing aromatic diamine with aromatic diacid halide; preparing a spinning dope by dissolving the aromatic polyamide in a solvent; and extruding the spinning dope through a spinneret, and sequentially passing the spinning dope through an air gap, a coagulation bath filled with a coagulation solution, and a coagulation tube having a jet opening, connected with the bottom of the coagulation bath, to obtain a filament wherein a distance from the upper surface of the coagulation solution contained in the coagulation bath to the jet opening of the coagulation tube is within a range between 10 and 35 mm.
priorityDate 2008-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4702876-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7488
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128554332
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID2749139
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7111
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID16720
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128421003
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID69917
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID129720493
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID127982453
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128051552

Total number of triples: 37.