Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aa0d7ed3f228505771ddba98288852f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_404204fda30ae6a279a341c5ba1f73bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8b8ec06fe8cc9b17e3554f6f3e3e3c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c98babf0d86f960b139cdb7401f3420f |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C1-1068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27B14-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27D27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27B14-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C32-0047 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27D3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27D11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-00 |
filingDate |
2008-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_66f22b7ecece213fed65d6612f87edf2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6da4f65ac0dce3d902ad701c8b29dc43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e81b17c72fccc2ea0d2b3b144a120e36 |
publicationDate |
2011-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011315920-A1 |
titleOfInvention |
Process for preparation of nano ceramic-metal matrix composites and apparatus thereof |
abstract |
A method to introduce ceramic particles into the liquid metal from the polymeric precursor route by in-situ process by cross-linking organic precursor into a hard polymer, this powder is crushed, and then added to the liquid melt for in-situ pyrolysis of the organic into the ceramic phase. The starting material, the organic, for the above process can be in the form of a liquid or a solid. If it is a solid it us usually dissolved into a solvent to create a liquid form. The organic is then cross linked either directly by a thermal process, by adding a catalyst, or by the well known sol-gel process into a hard polymer. It is this hard polymer which is then pyrolyzed into the high temperature ceramic material by the process outlined above. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103398593-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105420557-A |
priorityDate |
2008-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |