Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9628754e47c92578a6da8904d4e4252e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1aabade434911874658789bc899ce486 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_005033c11d2ba2ec38c6ce0d7ef0a1b8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8d85be21962972075d02c6624aa1080a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95585944cd76ddfb6dc33ed2a0b84403 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c32eaa624b45662b247afea68bf69094 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08786 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08782 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08797 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-16 |
filingDate |
2010-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f93c7cd2a95e5d8cd0b322a0368f564e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3fce3446a8f39a756178e1a919293da2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc9280b3b814069e126fe59d5301f095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fda3f6c2c8bada30875318b6b4cd622b |
publicationDate |
2011-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011305983-A1 |
titleOfInvention |
Release Agent for Toner, and Toner |
abstract |
The objectives of the present invention are attained with a release agent for toner that is obtained by grafting styrene compounds to an α-olefin polymer that conforms to the following conditions (a) and (b), wherein 70 mass % or more of the release agent is insoluble in 2-butanone when the release agent is dispersed at 25° C. into 2-butanone so that the mass ratio of the release agent to the dispersion is 15%. (a) The α-olefin polymer is to be produced by polymerization of at least one α-olefin monomer that has 16 or more to 36 or less carbon atoms. (b) The α-olefin polymer is to have a melting point between 30° C. or higher and 80° C. or lower, and has one peak temperature whose peak has the half-height width of 15° C. or less in a measurement of the melting behavior of the α-olefin polymer by means of differential scanning calorimetry. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015031707-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9606465-B2 |