abstract |
A continuous process for the ring-opening polymerisation of cyclic ester monomers to form aliphatic polyesters at a temperature between 100-240° C. which includes a) continuously providing cyclic ester monomer and polymerisation catalyst to a continuous mixing reactor, the reactor being operated at conditions effective for polymerisation to form a pre-polymerised reaction mixture, n b) continuously removing pre-polymerised reaction mixture from the continuous mixing reactor and continuously providing pre-polymerised reaction mixture to a plug flow reactor, the plug flow reactor being operated under polymerisation conditions, wherein the reaction mixture is polymerised to a degree of polymerisation of at least 90%, to form polymer, and n c) continuously removing polymer from the plug flow reactor. |