Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_22344ec8074a9ea45355eab882d0aee8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00612 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-0046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-0075 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00586 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L97-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J191-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D191-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-006 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J191-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 |
filingDate |
2011-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ad226e60f7ea09a0ea4831b48cae4f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53d25682736587940438c51acc3de529 |
publicationDate |
2011-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011259239-A1 |
titleOfInvention |
Bio-based adhesive material |
abstract |
A bio-based adhesive and method of making the adhesive replaces or serves as additives for asphalt, sealant, and polymers such as styrene-butadiene-styrene and atactic polypropylene in the manufacture of building or paving materials. The method includes steps of forming a mixture of oil comprising fatty acids group and optionally a powdered material; maintaining the oil-to-powdered-material weight ratio in the mixture between 1 to 0.00001 and 1 to 20; heating the mixture to a reaction temperature greater than 55 degrees Centigrade; maintaining the reaction temperature until the oil is polymerized; and, injecting air into the mixture while polymerizing the oil. The adhesive of this method comprises a renewable polymer and the powdered material. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021131029-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9475960-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9540544-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10907302-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9593211-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013171899-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10550574-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10934456-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023283451-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013295394-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107880785-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111607355-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111607355-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11598096-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013022823-A1 |
priorityDate |
2010-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |