Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a4d02db04ffddd8a36b020d51e6e8d34 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2207-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C4-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-30 |
filingDate |
2009-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f431107553fa35e0c6afcb716129bab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_048265232ddf5d332076509a9e22d04a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_83d000060e2787da4c21acdf16fa4446 |
publicationDate |
2011-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011217485-A1 |
titleOfInvention |
Method for coating a metal crucible element with a mixture of glass and ceramic |
abstract |
Angular sectors of a cylindrical wall of a crucible for vitrification of waste, built in steel and subject to high temperatures, are coated with a mixture of mainly glass and ceramic, the coating being subject to a heat treatment comprising a step between 650° C. and 850° C. so as to perform surface melting of the mixture filling the open porosity, improving dielectric strength and the cohesion of the coating, but without producing any excessive thermal expansion or oxidation of the substrate which would lead to fast flaking of the coating. |