http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011201769-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e3b3f4f8df8306f743faf2d4a4af65e1 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 |
filingDate | 2007-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e4f041eee1ef5730e04c996ea5956c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ecdf9687a5d7892abddbbba6cf91707a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6fbbecee49094eabd4f0e63160d0d22a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b7ed1d5738b026242de0510c6651cc2 |
publicationDate | 2011-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2011201769-A1 |
titleOfInvention | Copolymers Of Ethylene And At Least One Other 1-Olefin, And Process For Their Preparation |
abstract | Ethylene copolymers composed of ethylene units and units composed of at least one other 1-olefin whose density is from 0.940 to 0.955 g/cm 3 , whose vinyl end group content is at least 0.5 end groups, based on 1000 carbon atoms, whose tensile impact strength a tn , measured to ISO 8256 (1997)/1A at −30° C., is greater than or equal to 145 kJ/m 2 , and whose content of comonomer side chains per 1000 carbon atoms Cx is above a value defined via equation I, C x =128.7−134.62 d′ (I), where d′ is the density d of the copolymer in g/cm3, and a process for their preparation, and their use as blow-molded products. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011009580-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9228030-B2 |
priorityDate | 2006-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 99.