Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_77d28d79e0205338c9d3bda46d98ce39 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f6e105775cb4a95d56b41f8b755283b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4833c503c6eaf22f998d567584238c7b |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2201-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2301-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0278 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-00 |
filingDate |
2009-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e264b6d538c80e8634c8eabc96a3f26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c734dd77bd55c9781042da7768b187ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3358655c4e494398c83da280d80952e6 |
publicationDate |
2011-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011159274-A1 |
titleOfInvention |
Method of producing anti-glare film |
abstract |
The method for producing an anti-glare film ( 10 ) includes a coating solution preparation step in which at least two mutually incompatible resin materials ( 54 ) are dissolved in at least one solvent to prepare a coating solution containing particles; a coating step in which the coating solution is coated on a support ( 16 ) to form a coating layer ( 52 ); a particle migration step in which the particles are made to migrate to the air-liquid interface of the coating layer ( 52 ) to be eccentrically located on the surface of the coating layer ( 52 ); and a drying step in which the coating layer ( 52 ) is dried and phase-separated to form an anti-glare layer ( 58 ) and, at the same time, a low refractive index layer ( 60 ) comprising the particles on top of the anti-glare layer ( 58 ). |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113149452-A |
priorityDate |
2008-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |