Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2731e95721a6ea61aef77c93ff6f152f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d33ad995f0604f6d9710422652d595cc |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2495 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-212 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1317 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y99-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-2061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2218-155 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00853 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K5-0243 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-5041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-2456 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-87 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-52 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-06 |
filingDate |
2010-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93017dd9ed54de63546f5c5dc1c812f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b485b657213274ab34a9af1694d7832 |
publicationDate |
2011-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011159258-A1 |
titleOfInvention |
Electronic device housing and method for making the same |
abstract |
An electronic device housing includes a substrate and a nano titanium dioxide coating formed on the substrate is provided. The nano titanium dioxide coating has a thickness of about 10-100 nm. The nano titanium dioxide coating is formed of rutile crystals or composite crystals formed of rutile and anatase. A method for making the electronic device is also described there. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103317786-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109099538-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016227655-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8470419-B2 |
priorityDate |
2009-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |