abstract |
An optical film is provided and includes a cellulose ester and an acrylic resin. The mass ratio of the cellulose ester to the acrylic resin is 70/30 to 5/95, the total haze value of the optical film is 0.80 or less, the internal haze value of the optical film is 0.01 to 0.28, and the modulus of elasticity in the transverse direction of the optical film is 2,700 to 7,000 MPa. |