Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e757fd4fedc4fe825bb81b1b466a0947 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C35-0888 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2035-0833 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2035-0827 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C37-0003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00298 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00365 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C37-0067 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C37-005 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D11-00 |
filingDate |
2009-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1f1cb20def6523451f5ed39f9eb4c4a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1e9b453849b2517df6de4c1c67d6134 |
publicationDate |
2011-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011089590-A1 |
titleOfInvention |
Enhanced separation of injection molded microlenses for high volume manufacturing |
abstract |
A method and system for enhanced demolding of injection molded optical devices are disclosed. In one embodiment the system includes a metal moldplate without a coat of release layer and a curing device that generates high intensity pulses of UV light. The method includes: providing a moldplate made of a predetermined moldplate material; directly injecting optical material into cavities of a moldplate without a release layer; rapidly curing the injected optical material with high intensity pulses of UV light such that a predetermined optical device is formed; and separating the thus formed optical device from the cavities of the moldplate due to a differential thermal expansion between the optical device material and the moldplate material. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11787138-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015293269-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018273216-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11320591-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11318692-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020081697-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3867677-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10689134-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9995855-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021130239-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113167969-A |
priorityDate |
2009-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |