Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2707056d594790a62947ee030653e6f8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2331-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-919 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2978 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D03D13-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-605 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-05 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-60 |
filingDate |
2009-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67af989e6d0e8d66de1d8e9b810155dd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8143516e2f9af6d15e13c4059a884b91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e9ac4ffc8b3bc52a2e4d273fdc601ea http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a925fca5c923b9cc851968c2420e501 |
publicationDate |
2011-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2011045297-A1 |
titleOfInvention |
Para-aramid fiber and method of preparing the same |
abstract |
An aramid fiber and a method of producing the same is disclosed, which is capable of realizing high surface uniformity and improved tensile strength and elongation property, wherein the method comprises preparing an aromatic polyamide by polymerizing aromatic diamine with aromatic diacid halide; preparing a spinning dope by dissolving the aromatic polyamide in a solvent; and extruding the spinning dope through a spinneret, and sequentially passing the spinning dope through an air gap, a coagulation bath filled with a coagulation solution, and a coagulation tube having a jet opening, connected with the bottom of the coagulation bath, to obtain a filament wherein a distance from the upper surface of the coagulation solution contained in the coagulation bath to the jet opening of the coagulation tube is within a range between 10 and 35 mm. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113668089-A |
priorityDate |
2008-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |