http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011040022-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0db3f4eaff8e4e87f45f217371780f8e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 |
filingDate | 2009-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3bd641b9e5708f115440f971f5cbac59 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cd09ca846b9a180dfe9ffdaf5d56fed4 |
publicationDate | 2011-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2011040022-A1 |
titleOfInvention | Long-fiber-reinforced resin composition and molded article thereof |
abstract | A long-fiber-reinforced resin composition including the following component (A) and the component (B), the content of the component (A) being 50 to 90 wt % and the content of the component (B) being 10 to 50 wt %; and the content of reinforcing fiber contained in the component (A) being 20 to 60 wt % relative to the total amount of the fiber-reinforced resin composition: n [Component (A)]n a long-fiber-reinforced thermoplastic resin pellet including a thermoplastic resin, a modified polyolefin-based resin modified with an unsaturated carboxylic acid or its derivative and reinforcing fiber and satisfying the following (A-1) to (A-4):n n(A-1): the melt index of the thermoplastic resin (resin temperature: 230° C., load: 21.18N) is 100 to 250 g/10 min;n n(A-2): the relaxation time λ of the thermoplastic resin at an angular frequency ω=1 (rad/sec) calculated from the storage modulus G′ and the loss modulus G″ measured by means of a cone-and-plate rheometer is 0.1 (sec) or less;n n(A-3) the content of the reinforcing fiber is 40 to 70 wt %; andn n(A-4) the content of the modified polyolefin-based resin is 1 to 5 wt %;n n[Component (B)]n a polyolefin-based resin satisfying the following (B-1) and (B-2):n n(B-1) the melt index of the polyolefin-based resin (resin temperature: 230° C., load: 21.18N) is 20 to 70 g/10 min; andn n(B-2) the relaxation time λ of the polyolefin-based resin at an angular frequency ω=1 (rad/sec) calculated from the storage modulus G′ and the loss modulus G″ measured by means of a cone-and-plate rheometer is 0.23 (sec) or less. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015243975-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011263738-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011014454-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8420728-B2 |
priorityDate | 2008-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 123.