http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010308507-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00144 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-38 |
filingDate | 2010-06-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f42f890a180c183900900734a7530c78 |
publicationDate | 2010-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2010308507-A1 |
titleOfInvention | Method of producing resin molded article |
abstract | Provided is a method of producing a resin molded article which hardly involves the occurrence of optical distortion and of sink marks. The method of producing a resin molded article includes: a first step including pouring a polyfunctional (meth)acrylic monomer into a molding die and irradiating the polyfunctional (meth)acrylic monomer with radiant energy rays until a polymerization conversion degree reaches 1 to 10% to polymerize a part of the polyfunctional (meth)acrylic monomer; and a second step including heating the polymerized polyfunctional (meth)acrylic monomer after the first step in a state where the polymerized polyfunctional (meth)acrylic monomer is held in the molding die to further polymerize a remaining part of the polyfunctional (meth)acrylic monomer until the polymerization conversion degree reaches 60% or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013256927-A1 |
priorityDate | 2009-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 189.