Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b61dcd103d8773fdbc2c54babf807c33 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1393 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1352 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31855 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0083 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-06 |
filingDate |
2008-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_97947a70837b0d0d137a797983b6d30b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4ba7d4829d91f0e5621c69635c34193 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f8d8a7319af9fe46b3bc98f57d9b7ad |
publicationDate |
2010-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2010255236-A1 |
titleOfInvention |
Beta-nucleated propylene copolymer |
abstract |
Heterophasic propylene copolymer (HECO) comprising wherein the heterophasic propylene copolymer (HECO) is β-nucleated and the elastomeric phase has an intrinsic viscosity measured in tetraline at 135° C. of equal or below 4.0 dl/g. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9969859-B2 |
priorityDate |
2007-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |