abstract |
The present invention relates to a rubber composition for a sidewall, in which an effect on environments can be taken into consideration, provision for the future decrease of petroleum supply can be satisfied, and further, tear strength and flex crack growth resistance can be improved with favorable balance without increasing hardness, and a process for preparing the rubber composition. The rubber composition for a sidewall is characterized by comprising 15 to 60 parts by weight of silica and 2 to 20 parts by weight of a double bond-containing plasticizer on the basis of 100 parts by weight of a rubber component comprising 30 to 80% by weight of a natural rubber and 20 to 70% by weight of an epoxidized natural rubber. |