Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2001-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2001-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0034 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2301-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C41-24 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L1-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L1-14 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 |
filingDate |
2010-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2194492b1abca7330c0b0d4f00e0f45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da27378f964bcdcf0dd54e0d630c63c3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_abd397298687b54011901795aedbe9be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0b54c59052838cfb85559ae4dc9d701b |
publicationDate |
2010-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2010245730-A1 |
titleOfInvention |
Cellulose acylate film and method for producing same, retardation film, polarizer and image display device |
abstract |
A method for producing a cellulose acylate film, comprising casting a polymer solution that comprises a plasticizer having a number-average molecular weight of 200-10000 and a cellulose acylate to form a web; stretching the web having a residual solvent amount of 100-300% by mass in one direction at from −30° C. to 30° C.; drying the stretched web to reduce the residual solvent amount from 6-120% by mass to less than 12% by mass while controlling the surface temperature of the web so as not to reach 200° C. or higher; and stretching the resulting film at 60-200° C. in a direction different form the stretching direction of the first stretching. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107708965-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015032167-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11643477-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9855084-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9322955-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105690816-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019123843-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10605972-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10759872-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012173879-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10640577-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11248314-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11034776-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010143613-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018180787-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8425991-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105690782-A |
priorityDate |
2009-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |