Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_799b6c8cb40ea97102dceda7bfe7b5c7 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G41-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B13-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G23-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82B3-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G41-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G23-047 |
filingDate |
2009-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86d98ab7538196132d1b31f7509369d9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d71a34443aa28b0cf0ba720f8513493b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93852f7952b4160e2baff2e48081744d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f5568b9092bb45ba4f5860312b051d9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8927aa2b5f2e0e3898fdb3d23486ba5 |
publicationDate |
2010-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2010233074-A1 |
titleOfInvention |
Synthetic method of transition metal oxide nano-particles |
abstract |
Provided is a method for preparing transition metal oxide nanoparticles from a transition metal as a reactant. The method includes dissolving the transition metal into aqueous hydrogen peroxide to provide peroxi-metallate solution, and then adding a reactive solution containing an alcohol, water and an acid thereto to perform hydrothermal reaction. n More particularly, the method for preparing transition metal oxide particles includes: dissolving transition metal powder as a reactant into aqueous hydrogen peroxide to provide a peroxi-metallate solution with a molar concentration of transition metal of 0.001-0.2 M; adding a reactive solution containing an alcohol, water and an acid to the peroxi-metallate solution to provide a mixed solution; and subjecting the mixed solution to hydrothermal reaction to provide transition metal oxide nanoparticles. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015132640-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103818960-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102603003-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014061550-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11591235-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110078125-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9540249-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10090516-B2 |
priorityDate |
2009-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |