abstract |
One embodiment of the present invention provides a method for producing a stretched cellulose acylate film with an in-plane retardation, Re, of 100 nm or more and a relationship between the thickness direction retardation, Rth, and Re which satisfies Rth<(Re/2), by longitudinally stretching an unstretched cellulose acylate film in a longitudinal direction by pulling by means of a difference in circumferential velocity between a pair of rollers, wherein the method is characterized in that the cellulose acylate film is subjected to free-end uniaxial stretching to a longitudinal stretch ratio of 1 to 2 while the film is being heated in a heating oven installed between the pair of rollers at a stretching temperature in the range of Tc−10° C. to Tc+70° C., Tc being the crystallization temperature of the film, and with the temperature difference in the film width direction maintained within 10° C. |