http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010210446-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ee33b0e3e7398cf6fc957eeee59d510
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3418
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G4-1209
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-445
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3217
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3215
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3208
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3206
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3203
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3201
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-062
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-112
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C10-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C12-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-553
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-12
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-553
filingDate 2008-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c21b8b358a2777eefdcdfab454079505
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d89437c0f91aa13b53feb8d4c7828336
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_802a7a1f67dba1b06de82f8c63cfc57b
publicationDate 2010-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber US-2010210446-A1
titleOfInvention Low temperature co-fired ceramic powder and special raw material and use thereof
abstract The present invention relates to a ceramic powder and special raw material and use thereof. The raw material of the ceramic powder comprises 20-80 mass parts of SiO 2 , 10-50 mass parts of AlF 3 and 0-30 mass parts of regulator. The raw material for preparing the ceramic powder is mixed and crushed, followed by melted into liquid glass at 1200-1400° C., quenched to obtain the ceramic powder. The low temperature co-fired ceramic powder has the following advantages: low sintering temperature (750-850° C.) and controllable sintering shrinkage rate; the dielectric constant of the ceramic block prepared with the ceramic powder is adjustable between 4.5 and 10 (1 MHz), the dielectric loss is less than 0.002, the mechanical strength is high and the preparation process is simple. The ceramic powder may be used for electric devices such as ceramic substrate, resonator, etc. as well as in other microelectronic packaging.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102320822-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109626974-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113185270-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112521163-A
priorityDate 2008-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6660194-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5306338-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6107229-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5260476-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID702
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5318869
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512124
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419538410

Total number of triples: 43.