abstract |
The present invention relates to a method for preparing graphite layers, comprising the step of heating at least one monolayer with low-molecular weight aromatics and/or low-molecular weight heteroaromatics crosslinked in the lateral direction under vacuum or inert gas to a temperature of >800 K, and to graphite layers which are obtainable by this method. |