http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010160655-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c50c3ffd1c0826d6e6c68057eea7b7f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_27c6c789011f47c6439df36023d96988 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f9b64f47bf2a5a4a009fef134cf69365 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07D301-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C41-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C31-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07D301-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C209-00 |
filingDate | 2008-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d14608cca0290dd9c95588237b28fad3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_916318d02f7b75447281812cc87af2f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e74748d5d1790e978f5fb0a3fdc2d1ae |
publicationDate | 2010-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2010160655-A1 |
titleOfInvention | Method for improving the selectivity of a catalyst and a process for the epoxidation of an olefin |
abstract | A method for improving the selectivity of a supported highly selective epoxidation catalyst comprising silver in a quantity of at most 0.17 g per m 2 surface area of the support, which method comprisesn contacting the catalyst, or a precursor of the catalyst comprising the silver in cationic form, with a feed comprising oxygen at a catalyst temperature above 250° C. for a duration of up to 150 hours, and subsequently decreasing the catalyst temperature to a value of at most 250° C.; andn na process for the epoxidation of an olefin, which process comprisesn contacting a supported highly selective epoxidation catalyst comprising silver in a quantity of at most 0.17 g per m 2 surface area of the support, or a precursor of the catalyst comprising the silver in cationic form, with a feed comprising oxygen at a catalyst temperature above 250° C. for a duration of up to 150 hours, and subsequently decreasing the catalyst temperature to a value of at most 250° C. and contacting the catalyst with the feed comprising the olefin and oxygen. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103261177-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103261177-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2714670-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012078615-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114538592-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3749450-B1 |
priorityDate | 2003-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 172.