Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1f596cc14dde1c06a39c1cc12314f448 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1be00b68ebd48ca6773cc64c2e18faa2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2d6a3d4dd80c68296fef27e35915beb9 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S977-896 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F1-0545 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J13-0043 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-0545 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N33-553 |
filingDate |
2007-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_821e97de1c79d55afaf017a477d70ba9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b81c0c1cdd40e30d6f932a62616bdd04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_075f6a30a408f3fb553f55db301393a6 |
publicationDate |
2010-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2010159471-A1 |
titleOfInvention |
Process for production of colloidal gold and colloidal gold |
abstract |
It is an object of the present invention to provide a method for producing gold colloid having a targeted particle size, a sharp particle size distribution and a uniform and perfect spherical shape. The present invention relates to a method for producing gold colloid including a nucleation step of forming nuclear colloidal particles by adding a first reducing agent to a first gold salt solution; and a growth step of growing nuclear colloid by adding a second gold salt and a second reducing agent to the solution of the nuclear colloidal particles, characterized in that the growth step is performed at least once; a citrate is used as the first reducing agent and an ascorbate is used as the second reducing agent; and the addition of the ascorbate in the growth step is performed simultaneously with addition of the second gold salt. According to the method for producing gold colloid of the present invention, gold colloid having a sharp particle size distribution and a uniform and perfect spherical shape can be obtained. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102590521-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102539786-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11221330-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9581590-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102590520-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115575623-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102539773-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10203325-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102565409-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105067807-A |
priorityDate |
2006-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |