http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010148386-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad04f1f3296b8bfe5651585101e8182c
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_18aa81df225ad6d883c657a680776f6a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6fa7e3b53d2a205cbee0ac54a516c09e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_275b18ac2298543a81cacaf7f8072da4
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ead6a82ef93360813dd2f8bae800f789
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G2221-1639
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G2215-00987
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G21-1685
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G15-2035
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C73-00
filingDate 2008-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1687cf5ffb0a862f7bf73ef23340e47
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_970c01e4d336c93ccc1786d7d13305e9
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_25ce0e15ac1660c7b26abb065e29046c
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a4efa94b535e7b54a744cc65586ef390
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_197ac4f5e10f0155563054fa08f0451c
publicationDate 2010-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber US-2010148386-A1
titleOfInvention Method for refurbishing cylindrical members
abstract The present invention provides a method of resurfacing a cylindrical member in a printer having a fuser member that is externally heated by a heater roller. The method includes providing a cylindrical member having an outer surface of a high temperature fluorothermoplastic. When it is determined that the outer surface is in need of resurfacing, the fuser member is removed from the printer, and the cylindrical member is mounted in the place of the fuser member. The cylindrical member is rotated at a speed of at least 1 rpm while engaging the outer surface of the fuser member with the heating roller normally used to heat the fuser member at a pressure of at least 5 psi at a temperature of at least 10° C. below the fluorothermoplastic melting temperature for a time sufficient to resurface of the outer surface of the cylindrical member.
priorityDate 2008-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4224601-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007296122-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5485792-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007298251-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007298252-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008280035-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007298217-A1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6346
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128778904

Total number of triples: 31.