http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010048822-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 |
filingDate | 2007-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0fc233be3b6de1a8eff2b49b8c3be861 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a45cc5c8023821556f7435a8310069f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a77701d8b91e03bb566a3fe5ae94fa3e |
publicationDate | 2010-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2010048822-A1 |
titleOfInvention | Polypropylene resin composition |
abstract | There are provided a polypropylene resin composition and a molded article thereof, the composition comprising:n 60 to 85% by weight of a propylene homopolymer; and 15 to 40% by weight of an ethylene-α-olefin random copolymer containing 45 to 70 parts by mol of ethylene units, and 30 to 55 parts by mol of α-olefin units, and satisfying the following requirements (1) to (5), (1) the propylene homopolymer has a melting temperature of 163 to 170° C.; (2) the propylene homopolymer contains 0.01% or less of regio defects resulted from a 2,1-insertion and a 1,3-insertion in all propylene units; (3) the polypropylene resin composition has a ratio B/A of 0.9 or more, provided that A (% by weight) is an amount of the ethylene-α-olefin random copolymer contained in the polypropylene resin composition, and B (% by weight) is an amount of soluble parts in xylene at a room temperature contained in the polypropylene resin composition; (4) the ethylene-α-olefin random copolymer has a molecular weight distribution of 2.0 to 4.0; and (5) the ethylene-α-olefin random copolymer contained in the polypropylene resin composition has a shape of a particle, whose volume-average particle diameter is 1.0 μm or less, measured by observing a cross-section of a 0.5 mm-thick sheet with a transmission electron microscopy, the sheet being obtained by hot press-molding the above polypropylene resin composition at 190° C. for 3 minutes under a pressure of 35 kgf/cm 2 , provided that the cross-section of the above particle has a round shape. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013079470-A1 |
priorityDate | 2006-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 44.