abstract |
A fabrication method for a metal-base/polymer-resin bonded structured body according to the present invention includes the steps of: (1) applying, to a surface of the metal base, a solution containing an organometallic compound decomposable at 350° C. or lower; (2) baking the applied solution in an oxidizing atmosphere to form, on the surface of the metal base, a coating containing an oxide of the metal of the organometallic compound; (3) providing the polymer resin on the coating; and (4) hardening the polymer resin to provide the metal-base/polymer-resin bonded structured body. |