http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009124725-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3580d1ac047b3fa6c0502dbdeb1a4693 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 |
filingDate | 2006-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81c50812e7510e4749d76ae692516311 |
publicationDate | 2009-05-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2009124725-A1 |
titleOfInvention | Viscosity Modifier for Thermoplastic Polyester Resin, Thermoplastic Polyester Resin Composition Containing the Same, and Molding of the Composition |
abstract | The present invention provides a viscosity modifier (A) for thermoplastic polyester resin obtainable by polymerizing (a) 70 to 95% by weight of an aromatic vinyl monomer, (b) 5 to 30% by weight of an alkyl acrylate having an alkyl group with 1 to 8 carbon atoms, and (c) 0 to 10% by weight of other vinyl monomers copolymerizable with both; a viscosity modifier (A′) for thermoplastic polyester resin characterized by covering 100 parts by weight of polymer particles (A-1) with 0.5 to 30 parts by weight of polymer particles (A-2), the polymer particle (A-1) are obtained by polymerizing (a) 70 to 95% by weight of an aromatic vinyl monomer, (b) 5 to 30% by weight of an alkyl acrylate having an alkyl group with 1 to 8 carbon atoms, and (c) 0 to 10% by weight of other vinyl monomers copolymerizable with both and having a glass transition temperature of 60° C. or higher and a volume-average particle diameter of 50 to 500 μm, and the polymer particles (A-2) have volume-average particle diameter of 0.01 to 0.5 μm; and a thermoplastic polyester resin composition and a molded article containing the viscosity modifier. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014322487-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9732214-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115485313-A |
priorityDate | 2005-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 216.