http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009072432-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_34fbeb1e614ea098731393cc639cd372 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S428-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F110-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-6592 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F110-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-00 |
filingDate | 2008-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2587335ed47181c1dba3e5c1437bf870 |
publicationDate | 2009-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2009072432-A1 |
titleOfInvention | Biaxially-Oriented Metallocene-Based Polypropylene Films Having Reduced Thickness |
abstract | A polymer film having a thickness of 10 microns or less and improved barrier characteristics to both water vapor and oxygen is formed from a biaxially-oriented polypropylene film of isotactic polypropylene. The polypropylene is prepared by the polymerization of propylene in the presence of an isospecific metallocene catalyst. The film has a permeability to water vapor of less than about 2.5 g/m 2 day/25 μm and a permeability to oxygen of less than about 2200 cc/m 2 day/25 μm. The film also has a haze properties of less than about 1%. The polypropylene contains 0.1 to 1% 2,1 insertions and has an isotacticity of at least 96% meso pentads. The isotactic polypropylene thus produced is then extruded into a sheet that is biaxially-oriented by stressing the sheet in the transverse and longitudinal directions to a draw ratio of at least about 6:1 in the transverse direction, and at least about 4:1 in the longitudinal direction. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013295395-A1 |
priorityDate | 2007-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 124.