Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_311c752aa2bb526894fe8009c3053ec0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_af41fd5df5bddede1c416aed8c04e8d8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e43d4bf381d65432afdb25d6cd9d58db http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9c33006aa906da104d76b0a7f4cc75bf |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31551 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31935 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31786 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2367-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T156-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31511 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31504 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10853 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10871 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10761 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B38-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B17-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate |
2008-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c23cd3e539b195d60503ab89bff53d3c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92f9a8ada9bb3abf828624a977b84416 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_94ac59a721cf2daa56bf9222ff065c71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f0be96dcc36bec216a995bccdc686f3 |
publicationDate |
2009-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2009029174-A1 |
titleOfInvention |
Process for manufacturing glass/plastic laminates with improved optical quality |
abstract |
Provided is a process for manufacturing a glass/plastic laminate or a glass-less laminate having improved optical qualities. The process involves the use of a bi-layer film as a removable release liner. The bi-layer film comprises an inbound layer and an outbound layer. In the lamination process, the inbound layer is disposed adjacent to the plastic film outer layer and the outbound layer is disposed adjacent to a rigid cover plate. The polymeric material comprised in the outbound layer has a melting temperature that is higher than the temperature reached by the outbound layer in the lamination process. The melting temperature of the inbound layer is preferably at least 10° C. higher than the melting temperature of the outbound layer. Preferred bi-layer release liners include polyethylene/polypropylene films. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011048635-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9791601-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014311662-A1 |
priorityDate |
2007-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |