abstract |
The aqueous slurry is useful for chemical mechanical polishing a semiconductor substrate having a tantalum-containing barrier layer and copper interconnects. The slurry includes by weight percent, 0 to 5 oxidizing agent, 0.1 to 25 silica particles, 0.001 to 3 polyvinyl pyrrolidone, 0.02 to 5 weight percent imine barrier removal agent selected from at least one of formamidine, formamidine salts, formamidine derivatives, guanidine, guanidine derivatives, guanidine salts and a mixture thereof, 0.02 to 5 weight percent carbonate, 0.01 to 10 inhibitor for decreasing static etch of the copper interconnects, 0.001 to 10 complexing agent and balance water; and the aqueous slurry having a pH of 9 to 11. |