abstract |
In a packaging material for electrochemical cell, a thermally adhesive resin layer is configured of a resin having a propylene based elastomer resin in a propylene based resin. This propylene based elastomer resin is a copolymer composed of a constitutional unit derived from propylene and a constitutional unit derived from an α-olefin having from 2 to 20 carbon atoms; when the total sum of the constitutional unit derived from propylene and the constitutional unit derived from an α-olefin is defined as 100% by mole, contains 50% by mole or more of the constitutional unit derived from propylene; and is satisfied with (a) a Shore A hardness (ASTM D2240) of from 65 to 90, (b) a melting point of from 130 to 170° C., (c) a density (ASTM D1505) of from 860 to 875 kg/m 3 and (d) a glass transition temperature as measured by DSC of from −25° C. to −35° C. |