http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008241417-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b48583c52ec2fb1f6e5965af8562aaf2 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2405-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-0427 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-123 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-18 |
filingDate | 2007-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5eff5baa4c0b5b0a5280bbcf146e7988 |
publicationDate | 2008-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2008241417-A1 |
titleOfInvention | Process for manufacturing a flexible support for an electrophoretic medium |
abstract | A process for making a support for an electrophoretic medium comprising the steps of: applying an agarose coating to a corona treated polymeric film by transferring a layer of agarose solution onto a surface of the corona treated polymeric film. The pH of the agarose solution can be generally maintained between about 8 and about 11 and the concentration of the agarose solution can be generally maintained between about 0.1 and about 0.4% agarose by weight. The agarose powder used to make the agarose solution can be pre-treated by introducing a fresh reducing atmosphere above the agarose powder and exposing the agarose powder to a reducing atmosphere. The reducing atmosphere treatment may be repeated at least three times. |
priorityDate | 2007-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |