Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9bbab8cbb1a212ccede7631f1fdf1bc3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_69707a79247796838858819ae7f8e253 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1462 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1471 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24868 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B15-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-0086 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-0096 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B15-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 |
filingDate |
2007-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_12c2489b08e6296f4ba1a7a8b744d70c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_494d6d2c419359e5f9f5e07881434f99 |
publicationDate |
2008-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2008200333-A1 |
titleOfInvention |
Protective film temporarily lamination to electromagnetic wave shielding sheet, method for producing the same, and electromagnetic wave shielding sheet |
abstract |
The present invention is to provide an electromagnetic wave shielding sheet with a protective film that is temporarily laminated on a copper mesh layer for shielding electromagnetic waves, the electromagnetic wave shielding sheet is not discolored even after long-term use, especially at high temperature and high humidity, while the protective film exhibits appropriate adhesion properties. To achieve the object, there is provided an electromagnetic wave shielding sheet comprising a transparent substrate, at least a copper mesh layer provided on one surface of the transparent substrate and a protective film temporarily laminated to the copper-mesh-layer-side surface, the protective film comprises a support and an adhesive layer containing a polymer having repeating units derived from an acrylic ester and/or a methacrylic ester on the support, and the amount of free organic acids in the adhesive layer is an amount which makes 10 or less the color difference ΔE L*a*b* of the copper-mesh-layer-side surface of the electromagnetic wave shielding sheet before and after the adhesive layer surface is laminated on the copper-mesh-layer-side surface and they are left for 200 hours in an atmosphere of a temperature of 60° C. and a relative humidity of 95%. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102112127-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9397343-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10757849-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11317548-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108349208-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009126984-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9000309-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8039074-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2009051258-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11672108-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10772219-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I652005-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11241862-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180096766-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013048862-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11497152-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8242670-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016085326-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010247877-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2022039303-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018376602-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8426749-B2 |
priorityDate |
2006-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |